Digital Library Publications

British Glass has the UK’s only dedicated library on glass technology, from raw materials to end product. We collect and catalogue materials from sources including scientific journals, trade press, conference proceedings, standard setting bodies and more.

Each month our library and information service answers hundreds of enquiries from members – providing hand-picked information to help them meet their business needs. We particularly specialise in providing:

  • worldwide legislation, regulations, standards and guidelines – such as heavy metals, decoration, food contact
  • statistics – eg import/export data and recycling rates
  • factory data – including types of glass manufactured, production capacities
  • technical information on glass manufacture, material science, production techniques, compositions, decoration
  • patents – including searches going back to the 19th century.

If there is something specific we can help with, email [email protected] 
If you're not a member, we may still be able to help. Get in touch to find out more.

You can search our online database of articles, view abstracts, and order copies of articles using the search function below.

View our latest abstracts

Thermal Shock Resistance Of Milk Bottles

C T Roland & H A Trebler
Special Glass

Life Of Glass Tumblers

H Nakamura
Special Glass

Industrial Tests On A Cast Chrome-Corundum Refractory

O N Popov Et Al
Special Glass

Glass Composition Calculations

R C Srivastava
Special Glass
or search our library below...

Ice Flower Glass.

Anon.
Primary Papers

The Fluorescence Of Atoms Near A Glass Surface

M.F.H. Schuumans
Primary Papers

The Flow Of Glass Under Constant Stress And Under Constant Strain

P.G. Migeotte And H.P.C. Vandecapelle
Primary Papers

The Flow Of Cold Glass

J.R. Bast And P.G. Migeotte
Primary Papers

Flow And Temperature Distributions In Forehearths For Glass Container Machnies: I, Temperature Measurements In A Green Glass Forehearth Channel And Modeling Of The Temperature Felds.

H. Franzel.
Primary Papers

Flow And Temperature Conditioning Of Glass For Container Manufacture

R.S. Arrandale
Primary Papers

The Flora Olomouc '83 Exhibition An Exposition Of Glass And Flowers

Z. Stefka
Primary Papers

'Flow Point' As Reference Temperature At The Glass Viscosity Of 105 Poises

Z. Haberle And J Reinis
Primary Papers

Effect Of Supercritical Fluctuations And Phase Seperation On The Viscosity Of Melts And Glasses In The System Pbo-B2O3-Al2O3

S.V. Nemilov Et Al
Primary Papers

Method For Measuring The Flow Point Of Glass

R. Howard.
Primary Papers