Glass Composition Calculations

This article examines calculations involved in glass manufacture under three headings: i) The calculation of batch to glass; ii) the calculation of glass to batch; and, iii) the calculation of corrections for the use of arbitrary amounts of foreign or off composition cullet.

Author
R C Srivastava
Origin
Banaras Hindu University
Journal Title
Glass Udyog 1981 10 415-20