Digital Library Publications

British Glass has the UK’s only dedicated library on glass technology, from raw materials to end product. We collect and catalogue materials from sources including scientific journals, trade press, conference proceedings, standard setting bodies and more.

Each month our library and information service answers hundreds of enquiries from members – providing hand-picked information to help them meet their business needs. We particularly specialise in providing:

  • worldwide legislation, regulations, standards and guidelines – such as heavy metals, decoration, food contact
  • statistics – eg import/export data and recycling rates
  • factory data – including types of glass manufactured, production capacities
  • technical information on glass manufacture, material science, production techniques, compositions, decoration
  • patents – including searches going back to the 19th century.

If there is something specific we can help with, email [email protected] 
If you're not a member, we may still be able to help. Get in touch to find out more.

You can search our online database of articles, view abstracts, and order copies of articles using the search function below.

View our latest abstracts

Thermal Shock Resistance Of Milk Bottles

C T Roland & H A Trebler
Special Glass

Life Of Glass Tumblers

H Nakamura
Special Glass

Industrial Tests On A Cast Chrome-Corundum Refractory

O N Popov Et Al
Special Glass

Glass Composition Calculations

R C Srivastava
Special Glass
or search our library below...

Synthesis Of Ultrafine Powders With Mullite-Zirconia Composition By The Sol-Gel Method

A M Gabrukh Et Al
Special Glass

Stress Relaxation, Creep Recovery, And Newtonian Viscous Flow In Silicon Nitride

D A Woodford
Special Glass

Mathematical Modelling For The Identification Of Defect Bubble Sources

J Ulrich Et Al
Special Glass

Formation And Properties Of Alkali Scandium Silicate Glasses

J E Shelby & S R Shelby
Special Glass

Cordierite Crystallization In Glasses Derived From The Ca0-Mg0-Al203-Si02 Quarternary System. Influence Of The Glass Composition (In Spanish)

J Vila Et Al
Special Glass

Low-Cost Flip-Chip Process For Monolithic Microwave Integrated Circuits And Optical Components

G Humpston Et Al
Special Glass

Short Range Order In Sodium Borosilicate Glasses Obtained Via Deconvolution Of 29Simas Nmr Spectra

G Bhasin Et Al
Special Glass

Spectral Absorption Properties Of Pr3+, Nd3+, Er3+, And Tm3+ Ions In Zinc Sodium Phosphate Glass

S V J Lakshman, A S Kumar
Special Glass

Repeated Indentation Effect On Lead Alkali And Sodalime Glass Under Subcritical Loads Prior To Crack Initiation

B Rajat Et Al
Special Glass

Thermodynamic Properties Of Lixv2O5 Glasses

V I Gavriluk
Special Glass