Zirconium Based Bulk Metallic Glasses. Part 4

Promising industrial applications of these new glasses, exploiting their outstanding properties, are presented in this paper. Applications are: Defence (KEP ammunitions) and space industries, luxury products (jewellery, watches), electronic casings (for mobile phones and PC), sporting goods (tennis rackets, golf clubs baseball bats) as well as cutting tools (knives, surgical blades). Some present research topics (new compositions, light alloys, composites, coatings) aiming at reducing production cost, optimising the properties and/or diversifying the applications of bulk metallic glasses are mentioned.

Author
M Bletry
Origin
Canada
Journal Title
Verres Dec 05 12-17
Sector
Special Glass
Class
S 3138

Request article (free for British Glass members)

Zirconium Based Bulk Metallic Glasses. Part 4
Verres Dec 05 12-17
S 3138
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.