Zero-Cement Refractory Castables

Zero-cement high alumina castables in the alumina-silicon carbide-carbon system can be appropriately dispersed by adding citric acid to shift the alumina isoelectric point toward acid pH values.

Author
I R De Oliveira Et Al
Origin
University Of Sao Carlos, Brazil
Journal Title
Am Ceram Soc Bull 81 12 2002 27-34
Sector
Refractories
Class
R 463