Zeolites Synthesized From Class F Fly Ash And Sodium Aluminate Slurry

A Class F fly ash was combined with a sodium aluminate slurry (3:1 Na:A1) in an attempt to synthesize zeolites from a highly alkaline waste stream. The rection was studied as a function of composition (3:2, 1:1, and 1:2 fly ash:slurry), time (1, 3 and 7 days), and temperature (80, 130 & 180 deg C). X-ray diffraction analyses of the products indicated that the fly ash and sodium aluminate had combined to form Zeolite A at 80 deg C, and NaP1 (a gismondene-type) and an unnamed hydroxysodalite-type at 130 & 180 deg C. The fact that the pH of the reactants decreased from initial values in excess of 13 to near neutral (7-9) after reaction signifies that the bulk of the sodium had been incorporated into zeolitic phases.

Author
M W Grutzeck & D D Siemer
Origin
Pennsylvania State University & Lockheed Idaho Tech Co, Usa
Journal Title
J Am Ceram Soc 80 9 1997 2449-2453
Sector
Special Glass
Class
S 1226

Request article (free for British Glass members)

Zeolites Synthesized From Class F Fly Ash And Sodium Aluminate Slurry
J Am Ceram Soc 80 9 1997 2449-2453
S 1226
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.