Zebra Boards Give Way To Roller-Wave Gauges

Years ago, the topic of roller wave measurement in architectural glass aroused little interest among glass makers and fabricators. Windows were small enough to make distortion in reflected images hardly noticeable under most conditions. More recently, as larger glass becomes common, fabricators have been relying on so-called Zebra boards to detect major flatness defects. These days, glass with minimal roller wave distortion is now a sign of premium product quality to most building professionals. Many glassmakers still use Zebra boards, which rely on a totally subjective evaluation of the degree of distortion. The result is glass slipping through that is not only out of specification but inconsistent from batch to batch. This paper looks at various inexpensive methods,developed by Strainoptic, for accurately measuring roller wave in flat glass.

Author
J M Feingold
Origin
Strainoptic Technologies, Usa
Journal Title
Glass 80 8 Sept/03 244
Sector
Flat glass
Class
F 1457

Request article (free for British Glass members)

Zebra Boards Give Way To Roller-Wave Gauges
Glass 80 8 Sept/03 244
F 1457
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.