Is Your Cold End Coating Up To Scratch?

There is much more to achieving good cold end coating than simply spraying rows of containers. It is important to have control of the whole process from the hot end coating hood and ware handling, to the actual application of the cold end spray itself, as explained in this article.

Author
Un-named
Origin
Unknown
Journal Title
Glass International Dec-Jan/2013 24-25