Xps And Sims Characterization Of Tin-Oxide Coatings On Glass

In this paper, x-ray photoelectron spectroscopy (XPS) and secondary-ion mass spectroscopy (SIMS) have been utilized to examine both sputter-deposited tin-oxide coatings on glass subsrates and commercial hot-end coatings on glass containers.