Xps Analysis Of Glass: An O1S Line Study (French)

Oxygens have been identified as a function of the nature of the elements to which they are bonded. The chemical shifts of O1s for current bonds in glasses have been measured and the values obtained allow the O1s peak to be decomposed according to the chemical composition of the glass and current hypotheses on glass structure.

Author
I Berthelot, P Leheude
Origin
Saint-Gobain Recherche Aubervilliers
Journal Title
Riv Staz Sper Vetro 1990 20 5 45-48
Sector
General
Class
G 542

Request article (free for British Glass members)