Xps Analysis Of Glass Fibre Coatings For Reinforcements

Glass fibres account for 95% of fibre reinforcements currently used in the composites industry, principally because of their highly attractive performance to price ratio. Many glass fibre reinforcement products are made at speeds that exceed 1000 m/min. Within milliseconds of forming and cooling, glass fibres are coated with a "sizing" by contacting an applicator roll that carries a layer of an aqueous dispersion of organic materials. The sizing pickup occurs over a contact distance of less than 10mm in about 0.5 ms. All this combines to make sizing development and application a major technological challenge to commercial glass fibre production. It also makes attaining the optimum coating composition and coverage a major challenge to the production of high performance composite materials.

Author
J L Thomason
Origin
Owens-Corning, Usa
Journal Title
The Glass Researcher 9 2 Spring 2000 14-15
Sector
Glass Fibre
Class
GF 245

Request article (free for British Glass members)

Xps Analysis Of Glass Fibre Coatings For Reinforcements
The Glass Researcher 9 2 Spring 2000 14-15
GF 245
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.