Xpar Seminar Focuses On Better Quality Control

Delegates from all over the world attended a seminar on quality control held at the Rexam Glass Moerdijk glass bottle plant in the Netherlands recently. The seminar was organised by infra-red hot-end inspection equipment supplier XPAR Vision, who currently have 20 of its dual and 150 of its single camera units operating in glassworks around the world, providing badly needed information at the hot end. This article reports on highlights from the seminar.

Author
Un-named
Origin
Unknown
Journal Title
Glass July 2006 20-21