X-Ray Photoelectron Spectroscopy Study Of The Germanate Anomaly In The Na20-Ge02 System

Photoelectron spectra of the O 1s and Ge 3d levels have been obtained from a series of Na20-Ge02 glasses of general formula xNa20.(1-x)Ge02(x=0.125, 0.175, 0.2 and 0.3) and from powders of quartz-like Ge02 and rutile-like Geo2.