X-Ray Fluorescence Spectrometry Of Ba And Ca In Src03 Raw Materials

This report has explored the possiblity of using an x-ray spectrometer to analyse the Ba and Ca contents in SrCO3 raw materials. Viewed from the experimental result this method can reach the same requirement as chemical analysis. This is a very quick analytical method. This report has briefly described the possibility of using high purity reagent to make standard sample for SrCO3 x-ray fluorescent analysis. The experiment shows that because of the difference between the sample made by high purity reagent and the actual chemical industrial product, a powder pelletising method is needed to eliminate the effect of grain size and homogeneity.

Author
L Zhingxin
Origin
Unknown
Journal Title
Proc 17Th Icg, Vol 3 October 1995, Beijing, China 753-757
Sector
Special Glass
Class
S 1221

Request article (free for British Glass members)

X-Ray Fluorescence Spectrometry Of Ba And Ca In Src03 Raw Materials
Proc 17Th Icg, Vol 3 October 1995, Beijing, China 753-757
S 1221
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.