X-Ray Diffraction And Solid State Nmr Studies Of The Growth Of Hydroxyapatite On Bioactive Calcia:Silica Sol-Gel Glasses

An advanced materials characterisation methodology has been used to examine systematically a range of sol-gel glass materials of contemporary biomedical interest.