Wrap: Glass Sand Scores On The Golf Course

New research in the UK for WRAP, shows that using a blend of processed sand (made from 100% recycled glass) & conventional sand offers performance & environmental benefits & is closer to traditional sand colour. WRAP says this is good news for golf club greenkeepers who are reluctant to use processed sand due to its natural green colour. To find the optimum colour & performance ratio, trials were undertaken by the Sports Turf Research Institute on behalf of WRAP. The trials compared different blends of sand & showed that the optimum ratio was a 50:50 blend. This ratio maintained processed sand's performance advantages such as firmer underfoot conditions & reduced plugging of the ball but also significantly reduced the green colouring. Earlier trials demonstrated that processed sand was ideal for use in a range of applications on the golf course.

Author
Un-named
Origin
Unknown
Journal Title
Glassonline News 20 May 2005
Sector
Container glass
Class
C 2681

Request article (free for British Glass members)

Wrap: Glass Sand Scores On The Golf Course
Glassonline News 20 May 2005
C 2681
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.