Wrap Funds Trials To Show Potential Of Recycled Glass

Grant funding totalling £1.2M has been awarded by WRAP and the Scottish Executive for large-scale operational trials aimed at demonstrating the commercial, technical and operational potential of recycled glass as a raw material. Building on R&D work commissioned by WRAP into the use of recycled glass in a range of applications, the trials are designed to enable industry to better understand the performance and operational benefits of using recycled glass, with the ultimate aim of a wider market uptake. Ranging from building products through to water filtration, the scope of the trials is wide, ranging from: grit blasting in the marine sector; brick and tile fluxing; water filtration in food/chemicals processing industry; artificial sports turf; golf course construction & maintenance; mortars, adhesives & cement repairs & block manufacture.

Author
Un-named
Origin
Unknown
Journal Title
Glassonline News 21/07/05 - See: www.Wrap.org.Uk
Sector
Container glass
Class
C 2768

Request article (free for British Glass members)

Wrap Funds Trials To Show Potential Of Recycled Glass
Glassonline News 21/07/05 - See: www.Wrap.org.Uk
C 2768
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.