World'S Tallest Building

Laminated glass windows with DuPont Butacite polyvinyl butyral (PVB) interlayer have been installed in the world's tallest bulding, Petronas Twin Towers, in Kuala Lumpur, Malaysia. At 451.9 metres, the 88-story twin towers are 8.9 metres higher than the previous record holder since 1974, the Sears Tower in Chicago.