The Working Of Flat Glass (In Italian)

Temperature measurements at various stages in the production of flat glass are described.

Author
H.Pape And L.Unger
Origin
Unknown
Journal Title
Vetro Inforazione 1981 (2) 15-18
Sector
Primary Papers
Class
PP 195