[Windshields] Safety Glass Experts: How To Improve Lamination Process Performance

Lamination defects typically represent no more than 1-2% waste from the production of laminated windshields. These figures are not particularly high, but the total cost of waste created by lamination defects internally and externally is such that lamination requires special attention in process development work. The complex nature of lamination processes and lamination defects requires process parameters to be individually adjusted according to the raw materials used, product design and processing equipment.

Author
Un-named
Origin
Unknown
Journal Title
Glass-Tech Int 4/2012 53-57
Sector
Flat glass
Class
F 3331

Request article (free for British Glass members)

[Windshields] Safety Glass Experts: How To Improve Lamination Process Performance
Glass-Tech Int 4/2012 53-57
F 3331
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.