When Less Glass Wall Thickness Becomes A Solution

This article highlights a case where using the same mould design, different results were achieved in terms of glass distribution. It is not the most common issue to fiend in a glass plant. However, for niche markets where the same bottle or jar is produced in different colours, this is something to consider from a technical perspective. The results will be different and have implications when budgeting the costs of production.

Author
H Remedios
Origin
Empakglass, Portugal
Journal Title
Glass International July-August 2015 78-79
Sector
Container glass
Class
C 5506

Request article (free for British Glass members)

When Less Glass Wall Thickness Becomes A Solution
Glass International July-August 2015 78-79
C 5506
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.