Wetting In An Electronic Packaging Ceramic System: Ii, Wetting Of Alumina By A Silicate Glass Melt Under Controlled Po2 Conditions

The wetting of polycrystalline alumina by a coloured, calcia-magneisa aluminosilicate glass was found to be dependent on temperature between 1300-1500 deg C, but independent of gas atmosphere effects.

Author
D A Weirauch Jnr
Origin
Elcoa Labs, Usa
Journal Title
J Am Ceram Soc 78 11 1995 2923-2928
Sector
Special Glass
Class
S 958

Request article (free for British Glass members)

Wetting In An Electronic Packaging Ceramic System: Ii, Wetting Of Alumina By A Silicate Glass Melt Under Controlled Po2 Conditions
J Am Ceram Soc 78 11 1995 2923-2928
S 958