Wet-Shotcrete For Refractory Castables

A systematic investigation has been conducted involving parameters that control the wet-shotcrete technique for refractory castables.

Author
R G Pileggi Et Al
Origin
University Of Sao Carlos, Brazil
Journal Title
Am Ceram Soc Bull 81 10 2002 51-56
Sector
Refractories
Class
R 455

Request article (free for British Glass members)

Wet-Shotcrete For Refractory Castables
Am Ceram Soc Bull 81 10 2002 51-56