Ways Of Reducing Heat Losses Through The Insulated Walls Of A Glass-Melting Oven

The design parameters and physical characteristics influencing temperature distribution and variation in glass tank furnaces with added insulation have been examined by menas of a computer programme for 200 model situations.

Author
B V Vazhenin Et Al
Origin
Ural Building Design Res Org, Rostov Building Cons Org
Journal Title
Glass And Ceramics 1988 45 1-2 57-59