Waste Minimisation In Cleaning And Pretreating Operations

Pre-treatment operations involving cleaners and conversion coating treatments generate wastes containing oils and greases, heavy metals, and high BOD/COD content. Several washer design techniques and modifications for minimising these generated wastes will be discussed in this paper.

Author
C G Galeas Jr
Origin
Technologies Group, Henkel Corp, Michigan, Usa
Journal Title
Cesp 66 Porcelain Enamal Inst Tech Forum 25 5 2004 119-136
Sector
Enamels
Class
E 114