Waste Heat Recovery From Regenerative Glass Furnaces

Processes that have been proposed or demonstrated for waste heat recovery from regenerative glass furnaces are reviewed.

Author
F J Nelson
Origin
University Of Toledo, Toledo, Ohio
Journal Title
Glass Industry Vol 73 May 1992 26-31, 50
Sector
General
Class
G 773a

Request article (free for British Glass members)