Tuff Temp Corp has developed a series of high temperature-resistant conveyor belts that have been engineered for the hottest, heaviest and most severe hot end applications. Known as Tuff Temp Blended Belting, due to the intimate blend of multiple specialty high temperature-resistant fibre, they have already proved to be the longest lasting and most durable high temperature belts currently available.