Furnaces in the glass industry suffer from refractory corrosion at specific positions. Knowledge of wall thickness of a furnace at the metal line is necessary information for a proper start of external cooling in order to prevent complete corrosion of refractory. An application of a non invasive method for residual wall thickness estimation is presented in this paper. Combination of modelling and experimental surface temperature record of a non stationary heat transfer is necessary in order to calculate the actual wall thickness. A formula was derived for a temperature dependent effective heat transfer coefficient needed for calculation. Sensitivity analysis proved that the method is robust en ought to get reliable results. The approach used was an example of reasonable exploitation of modelling in the glass industry.

Author
P Vrabel Et Al
Origin
Alexander Dubcek University, Slovak Republic
Journal Title
Glass Sci Technol 77 1 2004 25-30
Sector
Refractories
Class
R 533

Request article (free for British Glass members)

Wall Thickness Estimation Based On Modelling Nonstationary Heat Transfer In A Glass Furnace
Glass Sci Technol 77 1 2004 25-30
R 533
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.