Voltammetric Studies Of The Redox Behaviour Of Various Multivalent Ions In Soda-Lime-Silica Glass Melts

Square wave voltammetry is described and compared with cyclic voltammetry as a technique for investigating polyvalent elements in glass melts.

Author
C Russell, E Freude
Origin
Universitat Erlangen-Nurnberg
Journal Title
Phys Chem Glasses 1989 30 2 62-68
Sector
General
Class
G 238

Request article (free for British Glass members)

Voltammetric Studies Of The Redox Behaviour Of Various Multivalent Ions In Soda-Lime-Silica Glass Melts
Phys Chem Glasses 1989 30 2 62-68
G 238
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.