Volatilisation Of Molten Sodium Metaborate With Convection Of The Furnace Atmosphere

Standard models for describing convective mass transport are reviewed. Experiments on the volatilisation of sodium metaborate with varying flow rates of nitrogen over the melt are then reported. It is shown that, in these conditions, sodium metaborate volatilises without change in the conposition of the melt but that the rate of volatilisation is considrably affected by the shielding effect of the rim of the capsule containing the sample.

Author
M Cable And M H V Fernandes
Origin
University Of Sheffield & University Of Aveiro, Portugal
Journal Title
Phys Chem Glasses 39 4 1998 228-235
Sector
Special Glass
Class
S 1513

Request article (free for British Glass members)

Volatilisation Of Molten Sodium Metaborate With Convection Of The Furnace Atmosphere
Phys Chem Glasses 39 4 1998 228-235
S 1513
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.