Volammetric Investigations In Na2So4-Refined Soda-Lime-Silica Melts

The redox behaviour of sulphate-refined soda-lime-silica melts was investigated by voltammetric methods. The possibilities for quantitative in-situ determination of sulphur and iron are discussed.