In Vitro Test Of Bioglass-Ceramics

Ceramised soda-lime-silica glasses with phosphate additions were found to be bioactive. Solubility of the compositions increased with soda content. The effect of additions of alumina, lithia and potassium oxide on solubility and surface activity was determined.