In Vitro Evaluation Of A Novel Ph Neutral Calcium Phosphosilicate Bioactive Glass That Does Not Require Preconditioning Prior To Use

It is well known that bioactive glasses can cause a significant increase in pH due to the rapid release of calcium and/or sodium ions. Consequently, preconditioning of the glass is usually required prior to surgery to negate the effect of this sudden release of ions. However, preconditioning for several days is far from ideal and also preconditioning is not practical for novel organic/inorganic sol-gel hybrids currently being developed since the organic phase will start to hydrolyze and dissolve. This study describes a bioactive glass that dissolves without causing a significant change in pH from physiologically optimal values and requires no preconditioning prior to use.

Author
A Li Et Al
Origin
Inst Chemistry, Beijing, China
Journal Title
Int J Appl Glass Sci 8 2017 403-411
Sector
Special Glass
Class
S 4478

Request article (free for British Glass members)

In Vitro Evaluation Of A Novel Ph Neutral Calcium Phosphosilicate Bioactive Glass That Does Not Require Preconditioning Prior To Use
Int J Appl Glass Sci 8 2017 403-411
S 4478
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.