Vitrification As A Way Of Cleaning Up Polluted Soil: An American Experiment

The Lower Fox River in the USA was badly contaminated with heavy metals as well as organic wastes. A search for remedial measures threw up the possibility of vitrification of the contaminated sediments. This paper briefly outlines Minergy's proposal for a multi-phased study to determine the cost effectiveness and the effectiveness of this technology to destroy organic contaminants and immobilize inorganic contaminants. With the assistance of a grant from the US Energy Protection Agency, Minergy conducted the Glass Furnace Technology feasibility study, whose four phases were: Mineralogy and sediment characterisation; Crucible melt and preliminary design engineering; Pilot-scale sediment melt of de-watered dredge material; and, Full-scale facility construction.

Author
Un-named
Origin
Unknown
Journal Title
Kanch December/2001 5
Sector
Special Glass
Class
S 2337

Request article (free for British Glass members)

Vitrification As A Way Of Cleaning Up Polluted Soil: An American Experiment
Kanch December/2001 5
S 2337
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.