Vitrification Of Incineration Residues

This paper briefly explains what vitrification is. Far more than a stabilising process, it is a technique that uses very high temperatures, which modify the state of the residues. The end product is then transformed into a type of glass that is innocuous for the environment and can be re-used.

Author
A Borderes
Origin
Europlasma, France
Journal Title
Verre 6 4 2000 19-21