Vitrification Of High Molybdenum Waste

In the UK, the Sellafield site Waste Vitrification Plant (WVP) currently immobilises highly active liquors produced from reprocessing of spent nuclear fuel into a borosilicate glass. Future challenges for WVP include the washout of solids from the base of the waste storage tanks in preparation for decommissioning, which will result in high molybdenum feeds to the plant. Molybdenum has a low solubility in the standard alkali borosilicate frit used on WVP, but laboratory experimental work has led to the development of a new calcium borosilicate glass formulation which can incorporate up to 10 wt% molybdenum oxide without any detrimental phase separation. Vitrification of high molybdenum feeds using the new formulation has also been carried out, using non-active simulants, on the Vitrification Test Rig (VTR) which is a full scale working replica of a WVP processing line. This paper discusses the results of both the laboratory and full scale trials.

Author
B F Dunnett Et Al
Origin
Nat Nuclear Lab, Sellafield, Cumbria
Journal Title
Glass Technol 53 4 2012 166-171
Sector
Special Glass
Class
S 4176

Request article (free for British Glass members)

Vitrification Of High Molybdenum Waste
Glass Technol 53 4 2012 166-171
S 4176
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.