Vitrification And Peroperties Of The Glasses In Fluorophosphate Systems Contianing Compounds Of 3D Elements

The glass formation region in flurophosphate systems containing CoO, MnO, NiO and NiF2 have been investigated. Optical spectra of the transition metal ions in the glasses have been measured.