Vital Statistics Of Forehearth Operation

In this article, John McMinn of Swinton-based Forehearth Services Ltd, discusses the benefits of forehearth audits. In terms of forming problems and ware rejection, the design and operation of the forehearth are highly significant factors in the productivity of a glass plant. Forehearth audits determine the performance of a forehearth and its associated subsystems.