Viscosity Temperature Relations In The Glass System Sio2-Al2O3-Na2O-K2O-Cao-Mgo In The Composition Range Of Technical Glasses

The chemical compositions of soda-lime glasses were expressed in molecular contents and in relation to 1.0 mole of silica. A balanced orthogonal latin square system was constructed with five variables at five levels each. A statistical analysis showed that if compositions are calculated on a molecular basis, the viscosity of glasses can be calculated from the composition with good accuracy. The effects of glass constituents on viscosity are linear with the molecular contents and additives. No interaction between the glass constituents could be established. So-called anomalies exist only if the glass composition is calculated in weight percentages. Three equations have been established for calculating the constants in the Fulcher equation from glass compositions.

Author
T Lakatos Et Al
Origin
Unknown
Journal Title
Glass Technology 13 3 1972 88-95 (Correction On P 160)
Sector
Primary Papers
Class
PP 151

Request article (free for British Glass members)

Viscosity Temperature Relations In The Glass System Sio2-Al2O3-Na2O-K2O-Cao-Mgo In The Composition Range Of Technical Glasses
Glass Technology 13 3 1972 88-95 (Correction On P 160)
PP 151
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.