Viscosity And Liquidus Temperature Of Ternary Glasses Close To The Eutectic Composition In The Cao-Al2O3-Sio2 System

Thermal properties of ternary glass-forming systems within the known CaO-Al2O3-SiO2 system were evaluated. The results discussed in this article may be useful for understanding and improving the modelling within the glass system.

Author
U Veit Et Al
Origin
Jena University, Germany
Journal Title
Int J Appl Glass Sci 7 3 Sept/2016 295-309
Sector
Glass Fibre
Class
GF 727