Viscosities And Working Region Predictions For Bismugh Aluminoborosilicate Glasses

Bismuth aluminosilicate glasses were prepared using a standard melt-quench technique, and the viscosity and thermal properties were measured and analysed. Electron microprobe analysis was used to examine glass homogeneity. Fragility was calculated based on Mauro-Yue-Ellison-Gupta-Allan model fits to the viscosity curves. The system is characterised by an open structure with high fragility (44-59).

Author
D Gardner Et Al
Origin
University Of Utah, Usa
Journal Title
Int J Applied Glass Science 10 2019 190-201
Sector
Special Glass
Class
S 4521

Request article (free for British Glass members)

Viscosities And Working Region Predictions For Bismugh Aluminoborosilicate Glasses
Int J Applied Glass Science 10 2019 190-201
S 4521
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.