Viscoelastic Effect Of Heat Treatment On The Fracture Toughness Of Metal-Particulate/Glass-Matrix Composites

The fracture toughness of a 90/10 glass-matrix/metal particulate composite was measured as a function of treatment temperature and hold time.

Author
T L Jessen, J J Macholsky
Origin
Us Naval Research Laboratory, Pennsylvania State University
Journal Title
J Am Ceram Soc 1989 72 11 2094-2097