Virtual Melting And The Generation Of New Glass Compositions

To find a glass composition whose properties will match a set of pre-assigned specific properties is a modern problem, especially when the requirements are unusual. A methodology as well as the preduction of compositions for six specific cases is described. The examples involve matching optical properties including refractive index and mean disperison with a pre-assigned optical specification. The term virtual melting process (VMP) is used to describe how the solutions are predicted.

Author
A K Nandi
Origin
Cgcri, India
Journal Title
Glass Technology 39 4 1998 134-137
Sector
General
Class
G 1882

Request article (free for British Glass members)

Virtual Melting And The Generation Of New Glass Compositions
Glass Technology 39 4 1998 134-137
G 1882
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.