The infrared absorption spectrum of vitreous silica is calculated using the quasi-cluster method for determining the eigen frequencies and atom vector displacements of rings composed of silicon-oxygen tetrahedra. The results show that the observed infrared spectrum of v-SiO2 can be successfully explained by the existence in the glass of puckered 4 and 6-membered rings as well as of a small amount of 3-membered planar rings.

Author
B D Mihailova Et Al
Origin
Bulgarian Acad Of Sci, Sofia
Journal Title
Chimica Chronica, New Series 23 1994 277-282
Sector
Special Glass
Class
S 910

Request article (free for British Glass members)

Vibrational Spectra Of Silicate Glasses Modelled On The Basis Of Sio4-Ring Structures
Chimica Chronica, New Series 23 1994 277-282
S 910
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.