Verlipack - Problems Return

Glass bottle manufacturer Verlipack of Belgium, which employs 400 people, is once again in a serious financial predicament. The company, in which German group Heye Glasfabrik has a stake, has consolidated losses well in excess of the BFr365m calculated in February. Observers attribute this "more than alarming" situation to an oversaturated market, causing prices to plummet in the last six months, as well as to serious management problems.

Author
Un-named
Origin
Unknown
Journal Title
Gmpa 2/98 37
Sector
News Items
Class
N 346

Request article (free for British Glass members)

Verlipack - Problems Return
Gmpa 2/98 37
N 346
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.