Various Scale Levels Of The Gel-To-Glass Transformation

The gel-to-glass transition in SiO2 xerogels prepared by inorganic sol-gel synthesis are studied.

Author
A Chmel Et Al
Origin
Academy Of Sciences Of Russia, St Petersburg
Journal Title
J Am Ceram Soc 76 6 1993 1563-1567