The Variation In Refractive Index And Density Across Two Sheets Of Window Glass

Two panes of glass, 3ft x 2ft, have been examined for heterogeneity. The density and refractive index of variously sized samples of glass were measured over a pane using a number of different methods. The results obtained from each method are compared with the experimental error and it is shown that a variation across a pane of glass is detectable using small fragments of glass by either density or refractive index measurement. In addition, the Becke line method for the determination of the refractive index of small fragments of glass has been studied. Different immersion liquids have been investigated and the precision of different instruments is shown.

Author
M D G Dabbs & E F Pearson
Origin
Home Office Central Research Est, Uk
Journal Title
J Forensic Sci Soc 10 1970 139-148
Sector
Primary Papers
Class
PP 105

Request article (free for British Glass members)

The Variation In Refractive Index And Density Across Two Sheets Of Window Glass
J Forensic Sci Soc 10 1970 139-148
PP 105
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.