Variability Of Optical Properties And Structure Of Glass

It is shown that that the network theory of glass formation may be broadened by the accessory enhancing effect of some asymmetry of electronic structure to explain the glass formation of compounds containing large amounts of lead oxide. The paper appeared originally in German in Acta Phys Austriaca 1949 3 4 405-417 and is reprinted to mark the author's 85th birthday.

Author
N J Kreidl
Origin
Unknown
Journal Title
Glastech Ber 1989 62 6 213-218
Sector
General
Class
G 257

Request article (free for British Glass members)

Variability Of Optical Properties And Structure Of Glass
Glastech Ber 1989 62 6 213-218
G 257
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.