Vaporisation Of Simple Substances Used In Glass Melting Iii. Vaporization Of Sodium Tetraborate Melt

The transpiration method was used to measure the density of molten borax vapours at 900 to 1150C in a nitrogen atmosphere and in nitrogen-water vapour mixtures. The results suggest a relatively small effect of water vapour on the density of borate vapours and indicate quasi-congruent vaporisation resulting from reaction of the melt with water vapour.

Author
J Hlavac, I Plasil
Origin
Institute Of Chemical Technology, Prague
Journal Title
Silikaty 1987 31 4 309-315