Vacuum Techniques For Thin Film Depostion On Polymetric Substrates

Some of the advantages of polymers as bulk material - such as chemical inertness, electrical insulating characteristics and low temperature processing - make them difficult to be coated. Vacuum deposition techniques overcome these limitations, increasing the field of application of this class of materials.